It is a bismuth-based eutectic fusible alloy made of four low-melting metals such as bismuth, tin, lead, and indium, without cadmium. It has a low melting point, can be melted in hot water, is easy to recycle and can be reused many times.

Description

We have unique advantages in many aspects, thus enhancing the market competitiveness of our bismuth indium tin ingot, high precision zinc alloy die casting machining parts, 136F eutectic fusible alloy bar and increasing the economic benefits of our enterprise. We abide by integrity and responsibility, and are willing to work hand in hand with people from all walks of life to create a harmonious and struggling bright future. With the concept of strivers, we strengthen the incentive mechanism for employees who work hard and contribute, so that excellent employees can share the fruits with the company and grow together.

Bismuth based alloy:

136F 58C

20220121154853ca40763c6ccf4bbca682af6b1383f214

Model

WOC-58C/136F

Product Name

58C 136F low melting alloy

Contained Elements

Bi, Sn, Pb, In

Color:

Grey

Melting Point

58℃/ 136℉

Density

9.01g/cm³

Eco-friendly

Non

Available Shape

Ingot/strip/plate/wire/ring/bead, etc

MOQ

5kg


Description:

It is a bismuth-based eutectic fusible alloy made of four low-melting metals such as bismuth, tin, lead, and indium, without cadmium. It has a low melting point, can be melted in hot water, is easy to recycle and can be reused many times. Mainly used for welding and temperature control of concealed sprinkler decorative cover; fusible alloy sprinkler thermal element(instead of glass ball);the production of heat-sensitive components, etc.



Picture

image003

image005

image007

image009

Single weight (about)


3kg/ingot


500g/pcs


25g/pcs


1kg/roll


To custom special specifications or specify the ratio, please feel free to contact us, we will reply as soon as possible.



We strictly control the quality of products, all V-57 (USA) / Gh2136 / GB/T 14992 / Gh136 / Precipitation Hardening Superalloy / have passed the quality supervision and inspection center inspection. We provide perfect services for the vast number of users in various fields around the world with a complete and effective application service system. As we have customer centric approach, we have made frequent innovations in our products that further provide maximum satisfaction to our clients. We also offer customized products to meet the specific demands of our clients to achieve customer satisfaction.

Hot Tags: 136f 58c bismuth tin lead indium alloy, China, manufacturers, factory, factory, customized, wholesale, buy, price, for sale, 136F 58C Bismuth Tin Lead Indium Alloy, 144F 62C Field s Metal Alloy, zinc die casting bike parts, in bi alloy solder, liquid gallium alloy, low melt alloy ingot